高质量文本数据驱动的命名实体识别加速镍基单晶高温合金材料知识发现 |
||||||||||||
| 刘悦, 姚文轩, 刘大晖, 丁琳, 杨正伟, 刘微, 于涛, 施思齐 | ||||||||||||
|
Named Entity Recognition Driven by High-Quality Text Data Accelerates the Knowledge Discovery of Nickel-Based Single Crystal Superalloys |
||||||||||||
| LIU Yue, YAO Wenxuan, LIU Dahui, DING Lin, YANG Zhengwei, LIU Wei, YU Tao, SHI Siqi | ||||||||||||
| 表2 不同模型在2个数据集上的表现(F1值) |
||||||||||||
| Table 2 Performance (F1-score) of different models on two datasets |
||||||||||||
|
||||||||||||