交叉包套轧制Ti-44Al-5Nb-1Mo-2V-0.2B合金的微观组织演化及力学性能 |
| 王秀琦, 李天瑞, 刘国怀, 郭瑞琪, 王昭东 |
|
Microstructure Evolution and Mechanical Properties of Ti-44Al-5Nb-1Mo-2V-0.2B Alloys in the Cross Hot-Pack Rolling Process |
| WANG Xiuqi, LI Tianrui, LIU Guohuai, GUO Ruiqi, WANG Zhaodong |
| 图9 不同轧制和退火热处理工艺下TNM-VB合金的室温和高温拉伸断口形貌 |
| Fig.9 Fracture morphologies of TNM-VB alloys in the UHPR (a, d), CHPR (b, e) processes, and annealed at 1200oC for 1 h, then furnace cooling (c, f) at room temperature (a-c) and 800oC (d-f) (Insets show the high magnified images) |
|