晶粒长大对高纯Al {111}/{111}近奇异晶界的影响
冯小铮, 王卫国, Gregory S. Rohrer, 陈松, 洪丽华, 林燕, 王宗谱, 周邦新

Effects of Grain Growth on the {111}/{111} Near Singular Boundaries in High Purity Aluminum
FENG Xiaozheng, WANG Weiguo, Gregory S. Rohrer, CHEN Song, HONG Lihua, LIN Yan, WANG Zongpu, ZHOU Bangxin
图3 再结晶高纯Al在500℃保温不同时间后的特定转轴晶界取向差分布图
Fig.3 Misorientation distributions of grain boundaries with specific rotation axis in high purity aluminum heated at 500oC for varied time after recrystallization
(a) <111> (b) <112> (c) <122>