晶粒长大对高纯Al {111}/{111}近奇异晶界的影响 |
| 冯小铮, 王卫国, Gregory S. Rohrer, 陈松, 洪丽华, 林燕, 王宗谱, 周邦新 |
|
Effects of Grain Growth on the {111}/{111} Near Singular Boundaries in High Purity Aluminum |
| FENG Xiaozheng, WANG Weiguo, Gregory S. Rohrer, CHEN Song, HONG Lihua, LIN Yan, WANG Zongpu, ZHOU Bangxin |
| 图1 经反复多向锻造和370℃再结晶后高纯Al显微组织的取向成像显微分析(OIM)图、晶界重构图及取向差分布图 |
| Fig.1 Microstructure analyses of high purity aluminum after multi-directional forging followed by recrystallization at 370oC (a) orientation imaging microscopy (OIM) (b) grain boundary networks (GBN) (c) misorientation distribution |
|