非均质Mn分布对淬火-配分钢微观组织和力学性能的影响 |
| 张超, 熊志平, 杨德振, 程兴旺 |
|
Effect of Mn Heterogeneous Distribution on Microstructures and Mechanical Properties of Quenching and Partitioning Steels |
| ZHANG Chao, XIONG Zhiping, YANG Dezhen, CHENG Xingwang |
| 图11 热膨胀曲线推导出的淬火阶段马氏体的转变曲线及一阶导数曲线 |
| Fig.11 Evolution of martensite fraction with quenching temperature deduced from the dilatation curves based on lever rule (a) and first order derivation of the transformation curves in Fig.9a (b) (QT—quenching temperature) |
|