非均质Mn分布对淬火-配分钢微观组织和力学性能的影响 |
| 张超, 熊志平, 杨德振, 程兴旺 |
|
Effect of Mn Heterogeneous Distribution on Microstructures and Mechanical Properties of Quenching and Partitioning Steels |
| ZHANG Chao, XIONG Zhiping, YANG Dezhen, CHENG Xingwang |
| 图1 以Mn配分珠光体为初始组织的淬火-配分工艺示意图 |
| Fig.1 Heat treatment schematic for partitioned pearlite-based quenching and partitioning (PPQ&P) process (WQ—water quench) |
|