M50轴承钢热变形过程中孔洞形成及演化机制 |
| 侯志远, 刘威峰, 徐斌, 孙明月, 时婧, 任少飞 |
|
Formation and Evolution Mechanism of Voids in M50 Bearing Steel During Thermal Deformation |
| HOU Zhiyuan, LIU Weifeng, XU Bin, SUN Mingyue, SHI Jing, REN Shaofei |
| 图11 热变形样品经850℃保温1 h后样品内部孔洞附近区域的SEM像及元素EDS线扫描分析 |
| Fig.11 SEM image (a), and EDS line scanning analyses from line AD (b) and EG (c) of the voids of the thermal deformation sample soaking at 850oC for 1 h (MZ, M'Z—matrix zones; VZ—void zone; HZ—healed zone; CZ, C'Z—carbide zones) |
|