Cu含量对管线钢耐微生物腐蚀性能的影响
曾云鹏, 严伟, 史显波, 闫茂成, 单以银, 杨柯

Effect of Copper Content on the MIC Resistance in Pipeline Steel
ZENG Yunpeng, YAN Wei, SHI Xianbo, YAN Maocheng, SHAN Yiyin, YANG Ke
表1 实验用钢的成分 (mass fraction / %)
Table 1 Chemical compositions of the steels
SteelCSiMnCuNbTiMoFe
1#0.020.010.071.340.040.0170.1Bal.
2#0.020.010.050.700.040.0170.1Bal.
3#0.020.010.05-0.040.0170.1Bal.