Cu含量对管线钢耐微生物腐蚀性能的影响 |
| 曾云鹏, 严伟, 史显波, 闫茂成, 单以银, 杨柯 |
|
Effect of Copper Content on the MIC Resistance in Pipeline Steel |
| ZENG Yunpeng, YAN Wei, SHI Xianbo, YAN Maocheng, SHAN Yiyin, YANG Ke |
| 图9 不同Cu含量管线钢在灭菌和接菌NS4溶液中浸泡14 d后的表面腐蚀产物形貌SEM像 |
| Fig.9 SEM images of Cu-bearing steels with different Cu contents immersed in sterile (a-c) and SRB inoculated (d-f) NS4 solutions for 14 d (Insets are the high magnification morphologies of the corrosion products on the steel surfaces. Red squares in the insets denote the element analysis locations) (a, d) 1# (b, e) 2# (c, f) 3# |
|