Cu含量对管线钢耐微生物腐蚀性能的影响 |
| 曾云鹏, 严伟, 史显波, 闫茂成, 单以银, 杨柯 |
|
Effect of Copper Content on the MIC Resistance in Pipeline Steel |
| ZENG Yunpeng, YAN Wei, SHI Xianbo, YAN Maocheng, SHAN Yiyin, YANG Ke |
| 图6 用于EIS拟合的等效电路模型 |
| Fig.6 Equivalent circuits model used to fit EIS data ( (a) equivalent circuit for one-time constant (b) equivalent circuit for two-time constant |
|