Cu含量对管线钢耐微生物腐蚀性能的影响 |
| 曾云鹏, 严伟, 史显波, 闫茂成, 单以银, 杨柯 |
|
Effect of Copper Content on the MIC Resistance in Pipeline Steel |
| ZENG Yunpeng, YAN Wei, SHI Xianbo, YAN Maocheng, SHAN Yiyin, YANG Ke |
| 图2 灭菌和接菌NS4溶液中不同Cu含量管线钢的开路电位随时间的变化 |
| Fig.2 Open circuit potential (EOCP) of Cu-bearing steels with different Cu contents in sterile (a) and SRB inoculated (b) NS4 solutions as a function of time (SRB—sulfate reducing bacteria, NS—no SRB, SCE—saturated calomel electrode) |
|