拉伸-扭转复合加载对镍基高温合金GH4169力学性能与变形机理的影响 |
|||||||||||||||||||
| 杨俊杰, 张昌盛, 李洪佳, 谢雷, 王虹, 孙光爱 | |||||||||||||||||||
|
Effect of Tension-Torsion Coupled Loading on the Mechanical Properties and Deformation Mechanism of GH4169 Superalloys |
|||||||||||||||||||
| YANG Junjie, ZHANG Changsheng, LI Hongjia, XIE Lei, WANG Hong, SUN Guang'ai | |||||||||||||||||||
| 表1 变形前后拉伸和扭转样品的晶格常数和位错密度 |
|||||||||||||||||||
| Table 1 Lattice parameters and dislocation densities for the undeformed specimen and those deformed PRTOR and PRTEN specimens under different loading modes |
|||||||||||||||||||
|
|||||||||||||||||||