中间层材料Fe和Nb对高强钛-钢复合管界面及剪切强度的影响
程磊, 张旭航, 韩盈, 程志诚, 余伟

Effects of Interlayer Materials Fe and Nb on Interfacial Shear Strength of Hot Extruded High-Strength Titanium-Steel Composite Pipe
CHENG Lei, ZHANG Xuhang, HAN Ying, CHENG Zhicheng, YU Wei
图8 Fe中间层样品920和970℃挤压后的组织特征,及Fe中间层970℃挤压态样品热处理后的组织特征和中间层析出特征
Fig.8 Microstructures of Fe-920oC (a) and Fe-970oC (b) samples, and microstructure of Fe-970oC-H (c) and corresponding precipitation state (d) (Arrows with green, blue, and red colors indicate the β-Ti grains, the original steel-Fe interface, and the newly formed zigzag interface after the hot extrusion process, respectively)