中间层材料Fe和Nb对高强钛-钢复合管界面及剪切强度的影响
程磊, 张旭航, 韩盈, 程志诚, 余伟

Effects of Interlayer Materials Fe and Nb on Interfacial Shear Strength of Hot Extruded High-Strength Titanium-Steel Composite Pipe
CHENG Lei, ZHANG Xuhang, HAN Ying, CHENG Zhicheng, YU Wei
图6 920和970℃挤压态和热处理态Fe、Nb中间层的界面硬度
Fig.6 Hardness distributions of Fe-970oC and Fe-970oC-H (a), Nb-920oC and Nb-920oC-H (b), Nb-920oC and Nb-970oC (c), and β-Ti layer in Nb-920oC-H (d)