中间层材料Fe和Nb对高强钛-钢复合管界面及剪切强度的影响
程磊, 张旭航, 韩盈, 程志诚, 余伟

Effects of Interlayer Materials Fe and Nb on Interfacial Shear Strength of Hot Extruded High-Strength Titanium-Steel Composite Pipe
CHENG Lei, ZHANG Xuhang, HAN Ying, CHENG Zhicheng, YU Wei
图5 Nb中间层920和970℃挤压态、热处理态的界面元素线分布特征及样品热处理后的界面形貌
Fig.5 Linear distributions of alloying elements (a, b, d, e) and interfacial microstructures (c, f) of samples with a Nb interlayer
(a) Nb-920oC (b, c) Nb-920oC-H (d) Nb-970oC (e, f) Nb-970oC-H