中间层材料Fe和Nb对高强钛-钢复合管界面及剪切强度的影响
程磊, 张旭航, 韩盈, 程志诚, 余伟

Effects of Interlayer Materials Fe and Nb on Interfacial Shear Strength of Hot Extruded High-Strength Titanium-Steel Composite Pipe
CHENG Lei, ZHANG Xuhang, HAN Ying, CHENG Zhicheng, YU Wei
图2 Fe中间层在920和970℃挤压后界面特征及合金成分面分布特征
Fig.2 Interfacial characteristics (a) and related phase distribution features (c) of the 920oC extruded sample with a Fe interlayer (Fe-920oC), and interfacial characteristics (b) and EDS mappings (d) of the 970oC extruded sample with a Fe interlayer (Fe-970oC)