表2 4种合金AQ和PA态的拉伸性能
Table 2 Tensile properties of the four alloys under the AQ and PA conditions
AlloyYS / MPaUTS / MPaEl / %Q / MPa
AQPAAQPAAQPAAQPA
0La97.2312.2172.4332.021.64.7372.6432.8
0.2La98.4318.8172.5341.424.57.4378.7471.1
0.4La111.1337.3203.4355.826.09.1415.6499.7
0.6La100.7316.3191.9337.728.210.2409.6489.0