稀土元素La对AlMgSi合金性能和微结构的影响
郑雄, 赖玉香, 向雪梅, 陈江华

Impacts of Rare Earth Element La on Properties and Microstructure of AlMgSi Alloys
ZHENG Xiong, LAI Yuxiang, XIANG Xuemei, CHEN Jianghua
表1 实验用4种合金的实际成分 (mass fraction / %)
Table 1 Chemical compositions of the four alloys used in the experiment
AlloyMgSiLaAl
0La0.730.76-Bal.
0.2La0.690.710.22Bal.
0.4La0.720.690.42Bal.
0.6La0.770.710.64Bal.