增材制造TiAl合金的研究进展 |
||||||||||||
| 陈玉勇, 时国浩, 杜之明, 张宇, 常帅 | ||||||||||||
|
Research Progress on Additive Manufacturing TiAl Alloy |
||||||||||||
| CHEN Yuyong, SHI Guohao, DU Zhiming, ZHANG Yu, CHANG Shuai | ||||||||||||
| 表3 Ti-47Al-2Cr-2Nb合金在不同加载方向下的室温拉伸性能[ |
||||||||||||
| Table 3 Room temperature tensile properties of Ti-47Al-2Cr-2Nb alloy under different loading directions[ |
||||||||||||
|
||||||||||||