增材制造TiAl合金的研究进展 |
||||||||||||
| 陈玉勇, 时国浩, 杜之明, 张宇, 常帅 | ||||||||||||
|
Research Progress on Additive Manufacturing TiAl Alloy |
||||||||||||
| CHEN Yuyong, SHI Guohao, DU Zhiming, ZHANG Yu, CHANG Shuai | ||||||||||||
| 表2 激光金属沉积(LMD)制造Ti-47Al-2Cr-2Nb合金的最佳工艺条件[ |
||||||||||||
| Table 2 Optimal process conditions for the manufacture of Ti-47Al-2Cr-2Nb by LMD[ |
||||||||||||
|
||||||||||||