增材制造TiAl合金的研究进展 |
| 陈玉勇, 时国浩, 杜之明, 张宇, 常帅 |
|
Research Progress on Additive Manufacturing TiAl Alloy |
| CHEN Yuyong, SHI Guohao, DU Zhiming, ZHANG Yu, CHANG Shuai |
| 图8 热处理EBM Ti-48Al-2Cr-2Nb合金的拉伸性能[ |
| Fig.8 Tensile properties of EBM Ti-48Al-2Cr-2Nb alloy subjected to heat treatment (HIP—hot isostatic pressing, DP—duplex, FL—fully lamellar)[ (a) yield strength (Rp0.2) (b) elongation (A) (Inset shows the locally enlarged curve) (c) ultimate strength (Rm) (d) stress-strain curves at room temperature |
|