增材制造TiAl合金的研究进展 |
| 陈玉勇, 时国浩, 杜之明, 张宇, 常帅 |
|
Research Progress on Additive Manufacturing TiAl Alloy |
| CHEN Yuyong, SHI Guohao, DU Zhiming, ZHANG Yu, CHANG Shuai |
| 图3 Ti-47Al-2Cr-2Nb合金热处理前后的SEM像[ |
| Fig.3 SEM images of Ti-47Al-2Cr-2Nb alloy[ (b) after heat treatment of 4 h at 1250oC followed by 4 h at 900oC |
|