增/降氧过程对高温合金粉末表面特性和合金性能的影响:粉末存储到脱气处理
郑亮, 张强, 李周, 张国庆

Effects of Oxygen Increasing/Decreasing Processes on Surface Characteristics of Superalloy Powders and Properties of Their Bulk Alloy Counterparts: Powders Storage and Degassing
ZHENG Liang, ZHANG Qiang, LI Zhou, ZHANG Guoqing
图7 不同窄粒度范围FGH96高温合金粉末在大气环境中(温度20℃、湿度40%~50%R.H.)存储不同时间的氧含量变化曲线
Fig.7 Curves of oxygen content of FGH96 superalloy powders with different narrow particle size ranges stored in ambient air (20oC, 40%-50%R.H.) for different time