增/降氧过程对高温合金粉末表面特性和合金性能的影响:粉末存储到脱气处理
郑亮, 张强, 李周, 张国庆

Effects of Oxygen Increasing/Decreasing Processes on Surface Characteristics of Superalloy Powders and Properties of Their Bulk Alloy Counterparts: Powders Storage and Degassing
ZHENG Liang, ZHANG Qiang, LI Zhou, ZHANG Guoqing
图6 不同窄粒度范围FGH96高温合金粉末的表面氧化膜的截面HAADF-STEM像和EDS面扫描图
Fig.6 Cross-sectional images of high-angle annular dark field scanning transmission electron microscopy (HAADF-STEM) (left) and energy dispersive spectrum (EDS) elemental mapping (right) on surface oxide layer of FGH96 superalloy powders with different particle size ranges
(a) 0-15 μm (b) 150-180 μm