激光增材修复单晶高温合金的热裂纹形成机制 |
| 卢楠楠, 郭以沫, 杨树林, 梁静静, 周亦胄, 孙晓峰, 李金国 |
|
Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys |
| LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo |
| 图5 裂纹源区域局部取向差(KAM)分布图 |
| Fig.5 Kernel Average misorientation (KAM) map of the crack initiation region |
|