激光增材修复单晶高温合金的热裂纹形成机制 |
| 卢楠楠, 郭以沫, 杨树林, 梁静静, 周亦胄, 孙晓峰, 李金国 |
|
Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys |
| LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo |
| 图4 裂纹源区域组织形貌及取向特征 |
| Fig.4 Morphology and orientation characteristics of the crack initiation region (a) back scattered electron (BSE) image of the crack initiation region (b-d) inverse pole figures (IPFs) along the X (b), Y (c), and Z (d) directions, respectively |
|