BAI Jiaming, LIU Jiantao, JIA Jian, ZHANG Yiwen
表1 GNPM01、FGH4098[24]和FGH4096[24]合金的化学成分 (mass fraction / %)
Table 1 Chemical compositions of GNPM01, FGH4098[24], and FGH4096[24] alloys
AlloyCCoCrMoWAlTiNbTaHfNi
GNPM010.0616.010.02.55.03.23.02.05.00.3Bal.
FGH4098[24]0.0520.613.03.82.13.43.70.92.4-Bal.
FGH4096[24]0.0313.015.84.334.142.263.880.82--Bal.