高W高Ta型粉末高温合金的蠕变性能及溶质原子偏聚 |
白佳铭, 刘建涛, 贾建, 张义文 |
Creep Properties and Solute Atomic Segregation of High-W and High-Ta Type Powder Metallurgy Superalloy |
BAI Jiaming, LIU Jiantao, JIA Jian, ZHANG Yiwen |
图6 650℃、980 MPa蠕变断裂后FGH4098合金中微孪晶附近的STEM-LAADF像、STEM-HAADF像及EDS元素面分布图 |
Fig.6 STEM low-angle annular dark field (LAADF) image (a), and STEM-HAADF image and corresponding element EDS mapping (b) along MTs in FGH4098 alloy after creep rupture at 650oC and 980 MPa |
![]() |