两种高代次镍基单晶高温合金热机械疲劳中的再结晶行为 |
| 赵鹏, 谢光, 段慧超, 张健, 杜奎 |
|
Recrystallization During Thermo-Mechanical Fatigue of Two High-Generation Ni-Based Single Crystal Superalloys |
| ZHAO Peng, XIE Guang, DUAN Huichao, ZHANG Jian, DU Kui |
| 图5 第三代和第四代高温合金孪晶片层附近沿[1 |
| Fig.5 BF-STEM image of paralleled twin lamellae for the third-generation single crystal superalloy (a) and HAADF-STEM image of paralleled twin lamellae and schematic illustration (inset) for the fourth-generation single crystal superalloy (b) from the [1 |
|