新型钴基高温合金中W元素对蠕变组织和性能的影响
陈佳, 郭敏, 杨敏, 刘林, 张军

Effects of W Concentration on Creep Microstructure and Property of Novel Co-Based Superalloys
CHEN Jia, GUO Min, YANG Min, LIU Lin, ZHANG Jun
表2 γ和γ'中滑移系开动阈值r0m和r0p (MPa)
Table 2 Initial threshold r0m and r0p of slip system for γ matrix and γ' precipitate, respectively
Alloyr0mr0p
8W18210
9W26235
10W30260