新型钴基高温合金中W元素对蠕变组织和性能的影响 |
| 陈佳, 郭敏, 杨敏, 刘林, 张军 |
|
Effects of W Concentration on Creep Microstructure and Property of Novel Co-Based Superalloys |
| CHEN Jia, GUO Min, YANG Min, LIU Lin, ZHANG Jun |
| 图10 γ基体和γ'相中位错运动的平均驱动力 |
| Fig.10 Mean driving forces of dislocation activity in γ phase (a) and γ' phase (b) |
|