新型钴基高温合金中W元素对蠕变组织和性能的影响 |
| 陈佳, 郭敏, 杨敏, 刘林, 张军 |
|
Effects of W Concentration on Creep Microstructure and Property of Novel Co-Based Superalloys |
| CHEN Jia, GUO Min, YANG Min, LIU Lin, ZHANG Jun |
| 图2 蠕变应变和蠕变速率曲线 |
| Fig.2 Simulated and experimental[ (a) creep strain (b) creep rate |
|