镍基高温合金疲劳裂纹急速扩展敏感温度及成因 |
| 江河, 佴启亮, 徐超, 赵晓, 姚志浩, 董建新 |
|
Sensitive Temperature and Reason of Rapid Fatigue Crack Propagation in Nickel-Based Superalloy |
| JIANG He, NAI Qiliang, XU Chao, ZHAO Xiao, YAO Zhihao, DONG Jianxin |
| 图1 疲劳裂纹扩展速率紧凑拉伸(CT)试样示意图 |
| Fig.1 Schematic of compact tension (CT) specimen for fatigue crack propagation test (unit: mm) |
|