镍基高温合金表面冲击强化机制及应用研究进展 |
| 王磊, 刘梦雅, 刘杨, 宋秀, 孟凡强 |
|
Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys |
| WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang |
| 图12 LSP和WLSP处理对IN718合金表面硬度分布的影响[ |
| Fig.12 Effect of LSP and WLSP on the surface microhardness distribution of IN718 alloy[ |
|