镍基高温合金表面冲击强化机制及应用研究进展 |
| 王磊, 刘梦雅, 刘杨, 宋秀, 孟凡强 |
|
Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys |
| WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang |
| 图9 单激光脉冲LSP处理后GH4586合金残余压应力的分布[ |
| Fig.9 Residual compressive stress distributions of GH4586 alloy treated with LSP of single laser pulse[ (a) surface layer along the diameter direction (b) depth direction from the surface to the inside |
|