镍基高温合金表面冲击强化机制及应用研究进展 |
| 王磊, 刘梦雅, 刘杨, 宋秀, 孟凡强 |
|
Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys |
| WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang |
| 图7 FGH96高温合金经不同表面处理后的表面形貌[ |
| Fig.7 Surface morphologies of FGH96 alloys with different surface treatments[ (a) mechanical polishing (b) laser shocking processing (LSP) |
|