表1 GH4169合金主要化学成分 (mass fraction / %)
|
Table 1 Chemical compositions of GH4169 alloy
|
|
| Grade | C | Cr | Ni | Co | Nb | Mo | Al | Ti | Fe |
|---|
| Normal | 0.015-0.060 | 17.00-21.00 | 50.00-55.00 | ≤ 1.00 | 4.75-5.50 | 2.80-3.30 | 0.30-0.70 | 0.75-1.15 | Bal. | | Premium | 0.015-0.060 | 17.00-21.00 | 50.00-55.00 | ≤ 1.00 | 5.00-5.50 | 2.80-3.30 | 0.30-0.70 | 0.75-1.15 | Bal. | | High purity | 0.012-0.036 | 17.00-19.00 | 52.00-55.00 | ≤ 1.00 | 5.20-5.55 | 2.80-3.15 | 0.35-0.65 | 0.75-1.15 | 16.00-19.00 | | Grade | Si | Cu | Mn | Mg | P | S | N | O | B | | Normal | ≤ 0.35 | ≤ 0.30 | ≤ 0.35 | ≤ 0.010 | ≤ 0.015 | ≤ 0.0080 | - | - | ≤ 0.006 | | Premium | ≤ 0.35 | ≤ 0.30 | ≤ 0.35 | ≤ 0.005 | ≤ 0.015 | ≤ 0.0020 | 0.01 | 0.0050 | ≤ 0.006 | | High purity | ≤ 0.35 | ≤ 0.30 | ≤ 0.35 | ≤ 0.003 | 0.007-0.015 | ≤ 0.0010 | 0.01 | 0.0025 | ≤ 0.006 |
|
|
|