高温合金锻件残余应力量化表征及控制技术研究进展 |
| 毕中南, 秦海龙, 刘沛, 史松宜, 谢锦丽, 张继 |
|
Research Progress Regarding Quantitative Characterization and Control Technology of Residual Stress in Superalloy Forgings |
| BI Zhongnan, QIN Hailong, LIU Pei, SHI Songyi, XIE Jinli, ZHANG Ji |
| 图10 GH4169合金γ"相变体选择行为对合金应力-应变关系的影响 |
| Fig.10 Effects of γ" phase variant selection behavior on the stress-strain relationship of GH4169 alloy (a) applied stress-strain curves for quasi-static in situ neutron tensile deformation (TA for tensile-aged, CA for compressive-aged) (b) evolution of hkl-specific lattice strain of the γ phase along the longitudinal direction[ (c) lattice strain evolution of the γ and γ" phases |
|