高温合金锻件残余应力量化表征及控制技术研究进展 |
| 毕中南, 秦海龙, 刘沛, 史松宜, 谢锦丽, 张继 |
|
Research Progress Regarding Quantitative Characterization and Control Technology of Residual Stress in Superalloy Forgings |
| BI Zhongnan, QIN Hailong, LIU Pei, SHI Songyi, XIE Jinli, ZHANG Ji |
| 图6 基于冷却场精准调控的高温合金残余应力控制装置(超级气冷)和实施效果示意图 |
| Fig.6 Schematic of residual stress control device for superalloys based on precise regulation of cooling field (super gas cooling) (a) and implementation effect (b) |
|