高温合金锻件残余应力量化表征及控制技术研究进展 |
| 毕中南, 秦海龙, 刘沛, 史松宜, 谢锦丽, 张继 |
|
Research Progress Regarding Quantitative Characterization and Control Technology of Residual Stress in Superalloy Forgings |
| BI Zhongnan, QIN Hailong, LIU Pei, SHI Songyi, XIE Jinli, ZHANG Ji |
| 图2 GH4169合金不同温度和应变速率下应力-应变关系实测与模拟结果对比[ |
| Fig.2 Comparisons between experimental measure-ments and finite element (FE) results at different temperatures and strain rates ( (a) |
|