镍基单晶高温合金的研发进展 |
||||||||||||||||||||
张健, 王莉, 谢光, 王栋, 申健, 卢玉章, 黄亚奇, 李亚微 | ||||||||||||||||||||
Recent Progress in Research and Development of Nickel-Based Single Crystal Superalloys |
||||||||||||||||||||
ZHANG Jian, WANG Li, XIE Guang, WANG Dong, SHEN Jian, LU Yuzhang, HUANG Yaqi, LI Yawei | ||||||||||||||||||||
表1 不同定向凝固工艺制备的单晶铸件组织对比 |
||||||||||||||||||||
Table 1 Microstructures of single crystal castings obtained by high rate solidification (HRS), fluidized bed cooling (FBC), and liquid metal cooling (LMC) |
||||||||||||||||||||
|
||||||||||||||||||||