涂层/高温合金界面行为及调控研究进展 |
| 宫声凯, 刘原, 耿粒伦, 茹毅, 赵文月, 裴延玲, 李树索 |
|
Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys |
| GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo |
| 图1 保温不同时间含涂层合金等效承载面位置示意图 |
| Fig.1 Sketch map of the effective load-bearing plane position in the coated superalloys with different thermal exposure time (IDZ—interdiffusion zone) |
|