聚变堆用W在等离子体作用下的辐照损伤行为研究进展 |
| 刘伟, 陈婉琦, 马梦晗, 李恺伦 |
|
Review of Irradiation Damage Behavior of Tungsten Exposed to Plasma in Nuclear Fusion |
| LIU Wei, CHEN Wanqi, MA Menghan, LI Kailun |
| 图14 W受到仅稳态等离子体辐照、仅瞬态高热流脉冲、顺序辐照、同时辐照后的表面形貌[ |
| Fig.14 Morphologies of W after different exposures[ (a) only steady state plasma exposure (b) only transient state high heat loads laser (c) consecutive exposure, laser induced transient heat loads on pre-exposed plasma (d) simultaneous exposure |
|