聚变堆用W在等离子体作用下的辐照损伤行为研究进展 |
| 刘伟, 陈婉琦, 马梦晗, 李恺伦 |
|
Review of Irradiation Damage Behavior of Tungsten Exposed to Plasma in Nuclear Fusion |
| LIU Wei, CHEN Wanqi, MA Menghan, LI Kailun |
| 图10 再结晶W表面晶内气泡的截面形貌[ |
| Fig.10 TEM morphologies of intra-granular blisters of recrystallized tungsten, H blisters respectively located in(100) plane (area 1) (a), (001) plane (area 2) (b), and (010) plane (area 3) (c); the locations of areas 1-3 in W near-surface (d)[ |
|