聚变堆用W在等离子体作用下的辐照损伤行为研究进展 |
| 刘伟, 陈婉琦, 马梦晗, 李恺伦 |
|
Review of Irradiation Damage Behavior of Tungsten Exposed to Plasma in Nuclear Fusion |
| LIU Wei, CHEN Wanqi, MA Menghan, LI Kailun |
| 图6 D等离子体辐照再结晶W的气泡和位错TEM像[ |
| Fig.6 TEM images of recrystallized W exposed to D plasma[ (a) original morphology of recrystallized W (b) intra-granular bubbles (Arrows show bubbles) (c-f) bubbles and surrounding dislocations |
|