聚变堆用W在等离子体作用下的辐照损伤行为研究进展 |
| 刘伟, 陈婉琦, 马梦晗, 李恺伦 |
|
Review of Irradiation Damage Behavior of Tungsten Exposed to Plasma in Nuclear Fusion |
| LIU Wei, CHEN Wanqi, MA Menghan, LI Kailun |
| 图5 D等离子体辐照后W的表面气泡和纳米泡(38 eV、1024 m-2·s-1、423 K、7 × 1026 m-2)[ |
| Fig.5 Surface bubbles and nanobubbles of W after D plasma irradiation (38 eV, 1024 m-2·s-1, 423 K, 7 × 1026 m-2)[ |
|