聚变堆用W在等离子体作用下的辐照损伤行为研究进展 |
| 刘伟, 陈婉琦, 马梦晗, 李恺伦 |
|
Review of Irradiation Damage Behavior of Tungsten Exposed to Plasma in Nuclear Fusion |
| LIU Wei, CHEN Wanqi, MA Menghan, LI Kailun |
| 图4 基于塑性变形机制的表面起泡模型[ |
| Fig.4 Surface blistering model based on plastic deformation mechanism[ |
|