新型低合金化高强Mg-0.2Ce-0.2Ca合金挤压过程中的组织演变机理 |
| 李景仁, 谢东升, 张栋栋, 谢红波, 潘虎成, 任玉平, 秦高梧 |
|
Microstructure Evolution Mechanism of New Low-Alloyed High-Strength Mg-0.2Ce-0.2Ca Alloy During Extrusion |
| LI Jingren, XIE Dongsheng, ZHANG Dongdong, XIE Hongbo, PAN Hucheng, REN Yuping, QIN Gaowu |
| 图10 挤压态Mg-Ce-Ca合金的局部取向差和晶界叠加处理图 |
| Fig.10 KAM + GB overlapped map for as-extruded Mg-Ce-Ca alloy (KAM—kernel average misorientation) |
|