新型低合金化高强Mg-0.2Ce-0.2Ca合金挤压过程中的组织演变机理 |
| 李景仁, 谢东升, 张栋栋, 谢红波, 潘虎成, 任玉平, 秦高梧 |
|
Microstructure Evolution Mechanism of New Low-Alloyed High-Strength Mg-0.2Ce-0.2Ca Alloy During Extrusion |
| LI Jingren, XIE Dongsheng, ZHANG Dongdong, XIE Hongbo, PAN Hucheng, REN Yuping, QIN Gaowu |
| 图1 Pandat计算Mg-0.2Ce-xCa合金的纵截面相图 |
| Fig.1 Vertical sectional phase diagram of Mg-0.2Ce-xCa alloy calculated by Pandat software (x—mass fraction of Ca (0~2%), T—temperature) |
|