偏析干预下体心立方金属再结晶织构竞争 |
| 常松涛, 张芳, 沙玉辉, 左良 |
|
Recrystallization Texture Competition Mediated by Segregation Element in Body-Centered Cubic Metals |
| CHANG Songtao, ZHANG Fang, SHA Yuhui, ZUO Liang |
| 图6 无Sb和含Sb的Fe-3%Si冷轧板再结晶早期和中期主要织构组分EBSD取向成像图 |
| Fig.6 EBSD orientation image maps of early (a, c) and middle (b, d) recrystallization stages without (a, b) and with (c, d) Sb addition (Grain boundaries of deformed grains are represented by white dotted lines. Invading and non-invading γ recrystallized grains are indicated by black and white arrows, respectively) |
|